Intumescent paint is a thin fire protection coating for structural steel that swells into a thick, insulating char when it is heated. On a normal day it looks like any other paint film, a few hundred microns to a few millimetres thick. In a fire it expands to many times that thickness and slows the rate at which the steel heats up, so the beams and columns keep carrying their load for the fire resistance period the building needs, typically 30 to 120 minutes.
The coating is simple to apply, but specifying it correctly is an engineering task. The thickness on each member depends on the fire period, the member’s shape and size, how many sides are exposed, and how hard the member is working. This guide explains each of those inputs, how the dry film thickness is set, how the paint system is built up for the UAE climate, and how it is inspected on site.
How intumescent paint works
Steel does not burn, but it loses strength as it heats. At around 550 °C, ordinary structural steel keeps only about 60% of its room-temperature yield strength, which is roughly the margin a typical member has between its design load in fire and its capacity. Unprotected, a light steel section can reach that temperature in 10 to 20 minutes in a standard fire.
Intumescent paint delays that point. When the coating reaches its activation temperature, usually around 200 to 250 °C, a chemical reaction releases gas inside a softening resin binder. The film foams and expands, typically 15 to 50 times its original thickness, into a carbon-rich char with many small closed cells. That char is a poor conductor of heat, and it insulates the steel for as long as it stays in place.
Three things decide how long the protection lasts:
- The thickness of the original film, called the dry film thickness (DFT)
- How quickly the steel section heats up, which depends on its shape and mass, expressed as the section factor
- The temperature the steel can reach before it fails, called the critical or limiting steel temperature
The structural design sets the last two. The paint manufacturer’s tested data then converts them into a DFT for every member.
Fire resistance periods: who sets them
The required fire resistance comes from the fire and life safety requirements for the building, not from the paint. In the UAE these come from the UAE Fire and Life Safety Code and the Civil Defence authority of the emirate, applied by the architect or the fire and life safety consultant according to the building’s use, height, area and sprinkler protection.
Typical ratings are written as R30, R60, R90 and R120, meaning 30, 60, 90 or 120 minutes of load-bearing resistance in the standard fire test. Elements that support other elements, such as columns and transfer beams, usually need at least the same rating as what they support. Some members may need no protection at all, for example in a single-storey building or where a fire engineering assessment shows they are not needed for stability.
Once the periods are fixed, the steel designer works out the two structural inputs for each member.
Critical steel temperature and member utilisation
The critical temperature is the steel temperature at which a member can no longer carry the load it has in the fire. It depends on how heavily the member is used in the fire limit state. A lightly loaded member can get hotter before it fails; a fully used one fails at a lower temperature.
Eurocode 3 Part 1-2 (EN 1993-1-2) gives the critical temperature θcr from the degree of utilisation μ0, the ratio of the design effect in fire to the design resistance at the start of the fire:
θcr = 39.19 ln[1 / (0.9674 μ0^3.833) − 1] + 482 (°C)
| Utilisation in fire, μ0 | Critical steel temperature θcr |
|---|---|
| 0.4 | about 620 °C |
| 0.5 | about 585 °C |
| 0.6 | about 554 °C |
| 0.7 | about 526 °C |
| 0.8 | about 496 °C |
The equation applies to members where buckling does not govern. For slender columns and beams with lateral-torsional buckling, the critical temperature is checked with the fire design rules for those modes. Under AISC 360 Appendix 4, the same idea is applied through the reduced yield strength and stiffness of steel at elevated temperature.
Many specifications simply use 550 °C for every member. That is conservative for lightly loaded members and can be unconservative for highly loaded columns and slender members. A steel designer who gives the utilisation of each member allows the paint manufacturer to use the real critical temperature, which often reduces the DFT on lightly loaded beams and keeps the right thickness on heavily loaded columns.
Section factor Hp/A (Am/V)
The section factor measures how fast a steel section heats. It is the heated perimeter of the section divided by its cross-sectional area, written Hp/A in British practice and Am/V in Eurocodes, in units of m⁻¹. A section with a large perimeter and little steel, such as a light beam, heats quickly and has a high section factor. A heavy, compact section heats slowly and has a low one.
Two choices affect the heated perimeter:
- Three-sided or four-sided exposure. A beam supporting a concrete slab on its top flange is heated on three sides, so the top face of the top flange is left out of the perimeter. A free-standing column is heated on all four sides.
- Profile or box protection. Intumescent paint follows the shape of the section, so the full profile perimeter is used. Boards form a box, and the box perimeter is used instead.
Approximate section factors for common sections:
| Section | Exposure | Hp/A (m⁻¹) |
|---|---|---|
| UB 457×191×67 beam | 3 sides, profile | about 171 |
| UB 457×191×67 beam | 4 sides, profile | about 193 |
| UB 457×191×67 beam | 3 sides, box | about 128 |
| UC 305×305×118 column | 4 sides, profile | about 122 |
| SHS 200×200×8 column | 4 sides | about 130 |
For a hollow section, Hp/A is close to 1/t, with t the wall thickness in metres, so an 8 mm wall gives about 125 m⁻¹. Hollow sections also heat differently from open sections, and intumescent products need separate tested data for them, often with a higher DFT for the same section factor.
In American practice the equivalent measure is W/D, the weight per unit length divided by the heated perimeter. The logic is the same, inverted: a higher W/D means a heavier, slower-heating section and a thinner coating.
How the dry film thickness is set
The DFT for each member is read from the manufacturer’s assessed loading tables, which come from fire tests on loaded and unloaded steel sections. In the UAE, products are normally assessed to BS 476 Parts 20 and 21, EN 13381-8 or UL 263, and must be approved by the Civil Defence authority for use.
For each member the table is entered with:
- The fire resistance period, for example R90
- The section type: open I or H section, or hollow section
- The member type and exposure: beam on three sides or column on four sides
- The section factor Hp/A
- The critical steel temperature
The result is a DFT, usually given in microns. Thicknesses range from a few hundred microns for R30 on heavy sections to several millimetres for R120 on light or hollow sections. Where the required DFT is beyond the range the product is tested for, the member needs a different product, a heavier section, or another form of protection.
The manufacturer or applicator issues a DFT schedule listing every member with its section, Hp/A, critical temperature, period and specified DFT. That schedule is what the paint inspector checks on site, so the member marks must match the steel drawings.
Types of intumescent paint
Intumescent coatings fall into three main families:
- Water-based thin-film coatings for dry interior steel. They have low odour and low emissions, which suits occupied buildings and fit-out, but they are sensitive to humidity during application and need a sealer coat where there is any risk of moisture.
- Solvent-based thin-film coatings for interior steel and covered areas with some humidity. They dry faster, tolerate a wider range of site conditions and suit shop application.
- Epoxy intumescent coatings for exterior steel, aggressive environments and hydrocarbon fire. They are thicker, harder and more durable, and are used in oil and gas plants, car parks and exposed structures. Hydrocarbon fire protection is tested to a much faster-rising fire curve, for example UL 1709, and needs products rated for it.
In the UAE the choice is driven by the exposure. Coastal sites and exposed steel fall in the higher corrosivity categories of ISO 12944, C4 or C5, where the paint system has to protect against corrosion for the life of the building as well as against fire.
Building up the paint system
Intumescent paint is one layer of a system, and each layer must be compatible with the next:
- Surface preparation: blast cleaning, normally to Sa 2½ to ISO 8501-1, with the surface profile the primer requires.
- Primer: a primer approved by the intumescent manufacturer and covered by its fire test data. Zinc-rich primers often need a tie coat before the intumescent is applied.
- Intumescent coat: applied in one or more coats to the specified DFT, within the maximum thickness per coat the manufacturer allows.
- Top coat: a sealer or decorative top coat where the steel is exposed to humidity, cleaning or ultraviolet light, or where a particular colour is required.
The specification should require a compatibility statement from the intumescent manufacturer for the full system. An untested primer or top coat can stop the intumescent from expanding properly in a fire.
Connections, bolts and special members
- Connections: the fire protection at a connection is normally applied to at least the highest DFT required for the members that meet there, extended a set distance along each member. Bolts, cleats and end plates are coated with the connection.
- Composite beams: the top flange of a composite beam is left unpainted where the shear studs are welded through the metal deck, and the voids between the deck profile and the beam are fire-stopped where the fire strategy requires. See our guide to shear studs in composite construction.
- Cellular and castellated beams: web posts between openings heat faster than a solid web, and the critical temperature depends on web-post buckling. These beams need DFT values from a method assessed for beams with web openings, which usually gives a higher DFT than a plain beam of the same size. See our cellular and castellated beam design service.
- Hollow section columns: these need products tested on hollow sections. Concrete-filled hollow sections can reach their fire rating with little or no protection, which is part of composite steel design.
- Bracing: bracing that is needed for the stability of the building in fire is protected to the same period as the frame it braces.
Shop or site application
Many projects in the UAE apply intumescent paint in the fabrication shop. Shop application gives controlled conditions, faster drying and less work at height, and the steel arrives on site finished. The trade-off is damage during handling and erection, so the specification should cover touch-up at connections, lifting points and bolted joints after erection.
Site application suits steel that is modified on site, very large members and refurbishment work. It depends on the weather: the steel surface must normally be at least 3 °C above the dew point, the relative humidity within the product limits, and the surface temperature below the maximum on the product data sheet, which matters on exposed steel in a UAE summer.
Inspection and acceptance
DFT is measured with an electronic gauge once each coat has dried. Readings are taken at set positions on the flanges and web of each member, at a sampling rate and with acceptance criteria set by the specification, typically by reference to ISO 19840 or SSPC-PA 2. A common criterion is that the average DFT on each member is not below the specified value and no single reading is below 80% of it, with thin areas built up and remeasured.
The inspection records, the DFT schedule, the product approvals and the applicator’s daily records form part of the handover file for the Civil Defence inspection.
Intumescent paint compared with other fire protection
| Method | Thickness on steel | Appearance | Programme | Typical use |
|---|---|---|---|---|
| Intumescent paint | 0.3 to about 5 mm | Follows the steel, can be a finished surface | Shop or site, no cladding needed | Exposed architectural steel, offices, malls, airports, hollow sections |
| Fire boards | 15 to 50 mm, boxed | Concealed, flat faces | Site, dry trade | Columns in finished interiors, heavy ratings |
| Sprayed cementitious | 10 to 50 mm | Rough, concealed | Site, wet trade | Concealed beams above ceilings, warehouses, plant areas |
| Concrete encasement or filling | 50 mm and more | Concrete finish | Part of the concrete works | Composite columns, high ratings |
Intumescent paint is usually the choice where the steel is part of the architecture, where the section is slender or curved, or where the programme favours shop application.
What the steel designer provides
Good fire protection starts with the structural information. For a fire protection package, the steel designer provides:
- The fire resistance period and exposure for each member, coordinated with the fire strategy
- The section factor for each member, three-sided or four-sided, profile or box
- The utilisation of each member in the fire limit state, or its critical temperature
- Member marks that match the DFT schedule and the shop drawings
- Details at composite beams, cellular beams, connections and bracing, so the protection can be applied as designed
Wrenze Steel provides this as part of our structural steel design service for real estate developers, architects and engineering consultancies, contractors and steel fabricators, and we review DFT schedules against the design for consultants as part of our steel design verification work.
Intumescent paint questions
How thick is intumescent paint?
It depends on the fire period, the section factor, the section type and the critical temperature. The dry film thickness ranges from a few hundred microns for 30 minutes on a heavy section to several millimetres for 120 minutes on a light or hollow section. The exact value for each member comes from the manufacturer’s assessed loading tables.
How long does intumescent paint protect steel?
It is specified for a fire resistance period, usually 30, 60, 90 or 120 minutes, set by the fire and life safety requirements for the building. Some products are tested for longer periods, often with high DFTs.
Can intumescent paint be used outdoors?
Yes, with a product rated for exterior use, usually an epoxy intumescent, and a suitable primer and top coat. Thin-film water-based products are for dry interior conditions only.
Why do some beams need a thicker coating than others?
Because they heat faster or fail at a lower temperature. Light sections with a high section factor, hollow sections, cellular beams and highly loaded members all need more protection than heavy, lightly loaded sections.
Does intumescent paint protect against corrosion?
The intumescent layer itself is not a corrosion protection system. Corrosion protection comes from the surface preparation, the primer and the top coat, chosen for the corrosivity category of the site and tested for compatibility with the intumescent.
Related
Structural steel design · Composite steel design · Cellular and castellated beam design · Steel design verification · Shear studs in composite construction
For fire protection inputs on your steel structure, contact our engineers.